Page 2.
United States Patent
Patent No.: X7875
To all to whom these Presents shall come:
Be it known that I, J. H. Geisenheimer of the City of New York in the State of New York have invented or discovered a new and useful improvement in the manufacture of Iron & Steel by the application of Anthracite coal in smelting iron ore into pig or cast iron in carbonating and refining Iron ore into malleable iron and in combining iron in a metallic state with a greater quantity of carbon, if bar iron, for steel, if white pig or cast iron, for a superior quality.
A correct account of which, drawn and signed by me, in the presence of a witness and attested by the signature of his name on the thirty first of August in the year of our Lord One thousand eight hundred and thirty one, was deposited and filed in the Patent Office on the fifth day of September in the same year One thousand eight hundred and thirty one — and that the following is a full and exact description of my said invention, discovery or improvement: viz.
I discovered first that Iron ore, raw or roasted can be may be decarboxylated & carbonated, and that so likewise, iron in a metallic state can and may be combined with a greater quantity of carbon than it possesses, by the sole use or application of anthracite coal, fully as well and as perfect as by the use or application of charcoal of wood —
For this purpose, the iron ore or the iron in a metallic state as the case may be, is mixed or stratified with dust or small pieces of Anthracite coal, in a smelting furnace similar to those used in converting bar iron into steel, or in a furnace of another construction, or in any other fit vessel. The
Page 3.
United States Patent
Patent No.: X7875
Iron ore or the ore fuel is thus successfully converted or altered, in order to be fused and reduce the acid materials therein contained from all kinds of atmospheric air, and is exposed for a sufficient length of time to such a degree of heat, which may be produced also by the use of Anthracite coal as fuel, as is necessary to effect the union of the iron in the ore or of the iron in a metallic state as aforesaid, as the case may be, with a sufficient proper or required quantity of carbon or coaly matter from the dust or small pieces of anthracite coal applied. Iron ore, so decacidated & carbonated can and may afterwards be smelted into pig or cast iron, the necessary flux being given, if the ore be not of such a nature as to require no flux. The smelting may be performed either in crucibles or in an air furnace, or in any kind of blast furnace with a blast appropriate to the anthracite coal used as fuel.
Iron ore so decacidated & carbonated can and may also be refined and converted into malleable iron, by subjecting it to such a process as is common in refining pig iron into malleable or bar iron, for which purpose anthracite coal may be also used as fuel.
By combining with carbon, from the dust or small pieces of anthracite coal as aforesaid, bar iron so usefully converted into steel, & white pig or cast iron of an inferior quality, into a quality greatly superior. By this discovery now described of a perfect decacidation and carbonation of raw or roasted iron ore by the sole use or application of anthracite coal I became convinced, that, pure anthracite is pure carbon in a very compact or dense state mixed with a small portion of earth and sometimes also with a small portion of oxide of iron, and knowing its great tenacity by which I mean not its cohesion when cold or in a low temperature but its aptness to run together in a moderately high temperature which can be overcome only by a greatly higher temperature, I was led to the further discovery of the whole mystery or the only true principle and manner, therefore unknown, to smelt or reduce iron ore into pig or cast iron of the best quality by the mere application of
Page 4.
United States Patent
Patent No.: X7875
anthracite coal exclusively as fuel, the iron ore being put or filled into the furnace now or reached as its particular nature will permit or require without being previously prepared by a separate process of desoxidation and carbonation as aforesaid, and I do hereby declare that the only thing or only true principle and manner, the great desideratum heretofore unknown, discovered by me to make the heat and the carbon of the Anthracite coal operate upon the iron ore and so smelt it, consists in applying in an appropriate blast furnace, a blast or a column, or stream, or current of air in or of such a quantity, velocity & density or compression as the compactness or density and the continuity of the Anthracite coal used, requires, that is to say, in a quantity, velocity & density or compression greater than is or would be required for charcoal of wood or coke of bituminous coal, and indeed so much, and in such a proportion, greater as the anthracite coal exceeds either the charcoal of wood, or coke of bituminous coal in compactness or density and in continuity.
In order to illustrate this principle, let it be supposed that the compactness or density and the continuity of the best charcoal of wood, be to the compactness or density and the continuity of the best coke of bituminous coal in proportion as one to two and a half, and let it be supposed, that the compactness or density & the continuity of the best coke of bituminous coal, be to the compactness or density & the continuity of the best Anthracite coal in proportion as two & a half to three and a half, then and in that supposed case, the quantity, velocity, and density or compression of a blast necessary & proper for such anthracite coal should be in proportion to the quantity, velocity and density or compression of a blast necessary and proper for such charcoal of wood, as three and a half to one and in proportion to the quantity, velocity and density or compression of a blast necessary and proper for such coke of bituminous coal as three and a half, to two and a half.
By this illustration, the true principle and manner of smelting iron ore with anthracite coal, is fully explained as above.
Page 5.
United States Patent
Patent No.: X7875
smelling as aforesaid, in applying an introducing into a blast furnace a blast in or of such a quantity of velocity and density or composition as the compactness or density and the continuity of the anthracite coal used, requires.
The blast may be of common atmospheric or of heated air; in either case the principle stated, remains unalterably the same. Heated air, I should prefer in an economical point of view.
In order not to be misunderstood, I observe again, that by the term, continuity, applying this term here to coal used in blast furnaces, I do understand and mean, not the cohesion of its particles out of the fire or in a low temperature, but its tendency or aptness to run and hold together or cohere in a certain high, but yet moderately high temperature, which is considered and overcome by increasing the temperature to a sufficiently higher degree.
That the construction of a blast furnace for the use of anthracite coal ought in width and height be proportioned accordingly, is reasonable; as a blast furnace for smelting iron ore with bituminous coal ought to be proportionally higher than is absolutely required for a blast furnace smelting iron ore with charcoal or wood; their respective widths being equal to a blast furnace for smelting iron ore with anthracite coal exclusively as fuel ought to a certain limit which future experience will best point out, be proportionally higher than a blast furnace for smelting iron ore with coke of bituminous coal as fuel, their respective widths being equal.
I would remark that the use of anthracite coal does not supersede the necessity or usefulness of applying an appropriate flux, where the nature of the iron ore used requires a flux; on the contrary, the smelting of earths met with, as even the most pure kind of anthracite coal requires a proportionate addition of limestone over and above the quantity required by the particular nature of the iron ore used.
What I claim as my discovery, is the following:
Page 6.
United States Patent
Patent No.: X7875
First, the application of anthracite coal exclusively or in part, in decacidating and carbonating iron ore as above specified and described.
Secondly, the application of anthracite coal exclusively or in part, in combining iron in a metallic state with a greater quantity of carbon, if bar iron or steel, if pig or cast iron, for a superior quality as above specified and described.
Thirdly, the smelting or reducing of iron ore so decacidated and carbonated by the application of anthracite coal as aforesaid, into pig or cast iron.
Fourthly, the refining or converting of iron ore so decacidated and carbonated by the application of anthracite coal as aforesaid, into malleable or bar iron.
Fifthly, the application of anthracite coal as fuel in smelting or reducing iron ore raw or roasted, did not prepared by a previous separate process of decacidation and carbonation as above described, into pig or cast iron.
I claim upon the principle and in the manner above stated by applying a blast in or of such a quantity, velocity and density or under such a pressure as the compactness or density and the continuity of the said coal used, requires exceeding the quantity, velocity and density or compactness not only of a blast, necessary and proper in the use of charcoal of wood as fuel, but also of a blast necessary and proper in the use of coke of bituminous coal as fuel, in such proportion as the compactness or density and continuity of the anthracite coal exceeds the compactness or density and the continuity of the charcoal of wood, or coke of bituminous coal, as above amply and fully described and illustrated.
Sixthly — I do not and do not claim an exclusive right of the use of heated air for any kind of fuel, nor do I claim to have a right to claim and do claim the use of heated air, applied upon and in connection with the said principle and manner described by me to smelt iron ore in blast furnaces.
Page 7.
United States Patent
Patent No.: X7875
with anthracite coal by applying a blast of fire in such a quantity, velocity and density or under such pressure, as the compactness or density and the continuity of the anthracite coal requires, as above amply and fully described and illustrated.
Dated at the city of New York on the twenty first day of November, One thousand Eight Hundred and Thirty Three.
Witnesses
Fairport Potter
H. K. Western
sig. Friedrich W. Geipenhain
[1824.209]
Published accounts: journal notice
Notice in the monthly list of patents, with remarks
Journal of the Franklin Institute, new ser., vol. 13 (1834), p. 395 · View the page
24. For Making Iron and Steel, by the use of anthracite coal; F. W. Geissenhainer, city of New York, December 19.
Remarks. The smelting of iron from the ore into pig, or cast iron; the carbonating and refining this into malleable iron; the combining iron in a metallic state with a greater quantity of carbon, if bar iron, for steel; if white pig, or cast iron, for a superior quality; are all to be effected under this patent, by means of anthracite coal. The patentee states that he has discovered the true principle, heretofore unknown, of applying anthracite to the purpose of smelting, &c.; and we sincerely hope that he may find his theory, or rather his practice, correct. The conversion of iron into steel may, he says, be effected by stratifying the iron with small pieces, or dust, of anthracite, in a cementing furnace, or in suitable vessels; anthracite being also used for heating the materials. The aptness of anthracite to fuse and run together in a moderately high temperature, the patentee denominates its continuity, and he claims to have discovered that this tendency is counteracted by a greatly increased temperature, which must be excited by applying in an appropriate blast furnace, a stream or portion of air, in such quantity, velocity, or density, as shall correspond with the excess of density, compactness, and continuity. Thus, if we suppose the density of charcoal, to the coke of bituminous coal, to be as two and a half to one; and of coke to anthracite, to be as two and a half to three and a half, the quantity, velocity, or density of the blast, must be in these proportions. " By this illustration," we are told that " the true principle and manner of smeltingiron ore with anthracite coal is fully explained. The claims are made under six distinct heads. First, the application of anthracite coal to the deoxidizing and carbonating of iron ore. Secondly, to the combining iron in a metallic state, with a greater quantity of carbon, if bar iron for steel; or if pig iron, to render it of a superior quality. Thirdly, the smelting or reducing iron so deoxidized and carbonated, by anthracite coal. Fourthly, the refining cast into bar iron, by the same material. Fifthly, the applying of the blast upon the principle specified, for the smelting of iron ore. Sixthly, the applying heated air to the purpose of smelting; not to the fact itself as a discovery, but to the using heated air in conjunction, or combination, with the process, or principle, of procedure, explained in the specification. We have thus given a general epitome of this specification; but think that the instrument itself is deficient in those practical details which are requisite to enable any one to follow the process described. It leaves an impression upon the mind that they have not been fully carried out by the patentee, or that he is not anxious to enable others to do so. This remark does not apply to the general principle of the American Patents for December, with Remarks. increase of the blast, although we think the defect pervades most of the operations alluded to.
About this record
- Patentee
- Jim Shaw's X-patent list
- Date
- the Name and Date index of patents, USPTO records, Jim Shaw's X-patent list
- Invention
- the Name and Date index of patents
- Listed in
- the Name and Date index of patents, USPTO records, Jim Shaw's X-patent list, the Journal of the Franklin Institute, Burke's List of Patents (1847)
- The residence comes from the Franklin Institute's journal.
- Burke's 1847 Patent Office list gives the same patent.